PRUITING®'s Honeycomb ceramic heat accumulation substrate are made of corundum-mullite, cordierite-mullite, cordierite, mullite, zirconia-mullite, carbo-corundum and so on with different hole shapes, such as square hole and hexagon hole, different wall thicknesses from 0.5mm to 5mm, and different figure specs.
Ceramic Honeycomb as the media of heat storage and heat exchange, has been widely applied in the fields of metallurgy, petroleum & chemical industry, electric power, boiler and so on.
It has high surface area,small resistance and thermal expansion,strong chemical corroding resistance,excellent thermal shock resistance.
A). Specification for cordierite heat accumulation substrate:
Chemical analysis
|
Comosition |
Value(%) |
|
Al2O3 |
28~38 |
|
SiO2 |
45~55 |
|
MgO |
12~14 |
|
Others |
<5 |
Physical properties
|
Index |
Unit |
Value |
|
Density |
g/cm3 |
1.7~2.0 |
|
Coefficient of heat expansion |
(X10-6K-1)(20-800℃) |
≤3.0 |
|
Specific Heat |
(J/Kg.k)(20~1000℃) |
900~1150 |
|
Thermal Conductivity |
(20~1000℃) |
1.2~1.8 |
|
Impact Thermal Resistance |
(℃/min) |
≥350 |
|
Max.Working Temp. |
℃ |
1320 |
|
Water absorption |
% |
15~25 |
Dimension and other physical properties
|
Dimension |
Quantity of channels |
Wall thickness |
Outside wall thickness |
Channel Width |
Void section |
Weight piece |
|
150×150×300 |
25×25 |
1.0mm±0.1 |
1.2mm±0.15 |
4.8-5.0mm |
67% |
3.2-4.2kg |
|
150×150×300 |
32×32 |
0.9mm±0.1 |
1.2mm±0.15 |
3.8-3.9mm |
61.6% |
3.7-4.7kg |
|
150×150×300 |
40×40 |
0.7mm±0.1 |
1.1mm±0.15 |
2.9-3.1mm |
64% |
3.6-4.6kg |
|
150×150×300 |
43×43 |
0.65mm±0.1 |
1.1mm±0.15 |
2.7-2.9mm |
62% |
3.7-4.7kg |
|
150×150×300 |
50×50 |
0.6mm±0.1 |
0.8mm±0.15 |
2.3-2.5mm |
61% |
3.8-4.8kg |
|
150×150×300 |
60×60 |
0.45mm±0.1 |
0.8mm±0.15 |
1.9-2.1mm |
63.4% |
3.6-4.6kg |
Contact: Amanda Wu
Phone: 18775376470
Tel: +8618775376470
Email: [email protected]
Add: No.26, Huangang Road, Konggang Industrial Park, Yubei District, Chongqing,China.